Vickers Indentation Fracture (VIF) modeling to analyze multi-cracking toughness of titania, alumina and zirconia plasma sprayed coatings D Chicot, G Duarte, A Tricoteaux, B Jorgowski, A Leriche, J Lesage Materials Science and Engineering: A 527 (1-2), 65-76, 2009 | 93 | 2009 |
Depth-sensing indentation modeling for determination of elastic modulus of thin films A Tricoteaux, G Duarte, D Chicot, E Le Bourhis, E Bemporad, J Lesage Mechanics of Materials 42 (2), 166-174, 2010 | 53 | 2010 |
Solid-state synthesis of mullite from spent catalysts for manufacturing refractory brick coatings F Vargas, E Restrepo, JE Rodríguez, F Vargas, L Arbeláez, P Caballero, ... Ceramics International 44 (4), 3556-3562, 2018 | 37 | 2018 |
Hydriding properties of an Mg–Al–Ni–Nd hydrogen storage alloy GI Duarte, LAC Bustamante, PEV De Miranda Scripta materialia 56 (9), 789-792, 2007 | 28 | 2007 |
Elaboración de recubrimientos cerámicos mediante proyección térmica por combustión a partir de residuos sólidos industriales E Restrepo, F Vargas, M López, R Cardona, G Duarte Matéria (Rio de Janeiro) 17, 1176-1185, 2012 | 17 | 2012 |
Evaluation and implementation of High Density Polyethylene liner: Alternative of solution to corrosion-wear problems in flowlines G Duarte, M Valera, M Manrique, M Mateus CT&F - Ciencia, Tecnología & Futuro 9 (1), 65 - 72, 2019 | 9 | 2019 |
Elaboration of ceramic coatings by flame spraying process from industrial solid waste E Restrepo, F Vargas, M López, R Cardona, G Duarte Matéria (Rio de Janeiro) 17, 1176-1185, 2012 | 2 | 2012 |
Magnesium based-alloys for hydrogen storage PEV De Miranda, GID Poveda, LA da Cunha Bustamante US Patent 9,017,603, 2015 | 1 | 2015 |
Sulfidation and Naphthenic Acid Corrosion of UNS S31603, UNS S31703 and UNS S44400 Series Stainless Steels in Crude Processing GID Poveda, EA Morantes, NEM Cajicá, DYP Ballesteros NACE CORROSION, NACE-2013-2517, 2013 | 1 | 2013 |
Evaluación del efecto protector de los depósitos formados por corrosión nafténica y sulfidación sobre acero al carbono y acero 5Cr-0,5Mo expuestos en fracciones de destilación … GD E Morantes, E Bohórquez, D Peña, M Mateus Revista de Metalurgia 53 (2), 9, 2017 | | 2017 |
Evaluation of protective effect of deposits formed by naphthenic corrosion and sulfidation on carbon steel and steel 5Cr-0.5 Mo exposed in atmospheric distillation fractions G Duarte, E Morantes, E Bohorquez, D Pena, M Mateus REVISTA DE METALURGIA 53 (2), 2017 | | 2017 |
Un facteur d'échelle en dureté pour représenter l'effet de taille en nano et en micro-indentation F Roudet, J Mendoza, G Duarte, J Lesage, D Chicot Matériaux & Techniques 96, 43-52, 2008 | | 2008 |
Hardness Length-Scale Factor to represent the nano and microindentation size effect F Roudet, J Mendoza, G Duarte, J Lesage, D Chicot MATERIAUX & TECHNIQUES 96, 2008 | | 2008 |
Un facteur d’échelle en dureté pour représenter l’effet de taille en nano et en micro-indentation Hardness Length-Scale Factor to represent the nano and micro-indentation size … F Roudet, J Mendoza, G Duarte, J Lesage, D Chicot | | |
REVESTIMENTOS RESISTENTES À CORROSÃO POR ÁCIDOS NAFTÊNICOS GI Duarte, EA Morantes, NE Mejía | | |
DESSORÇÃO DE HIDROGÊNIO DA LIGA Mg-5Al GID POVEDA, LADAC BUSTAMANTE, PEV DE MIRANDA | | |